Petromont 2100 Medium Density Polyethylene Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , MDPE
Manufacturer Petromont
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 2100 Medium Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Petromont HDPE 2100 is a medium density polyethylene blown film resin produced using the UNIPOL™ Process. This resin is designed specifically for blown film made by co-extrusion. It is commonly used in HDPE resins in applications where an improvement in the film resilience property is required, and with LLDPE where higher stiffness is required.Petromont HDPE 2100 has a broad molecular weight distribution. This, combined with its medium molecular weight and medium density, results in excellent processing characteristics at high extrusion rates with good flexibility and resilience. The excellent draw down characteristics permit production of high quality thin films
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Melt Flow 0.20 g/10 min
0.20 g/10 min
I<sub>2</sub>; ASTM D1238
20 g/10 min
20 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Tensile Strength at Break 32.0 MPa
4640 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.690 GPa
100 ksi
at 1% elongation; ASTM D790
Thermal Properties Metric English Comments
Melting Point 125 °C
257 °F
Petromont
Vicat Softening Point 116 °C
241 °F
ASTM D1525
Descriptive Properties Value Comments
Process Film