Material Notes:
Petromont HDPE 5000 is a high density polyethylene copolymer resin produced using the UNIPOL™ Process. This resin is intended for use in prime sheet and thermoforming applications such as arena boards, biscuit trays and panels.Petromont HDPE 5000 is an intermediate molecular weight hexene modified resin with a narrow molecular weight distribution offering an excellent combination of rigidity (stiffness), toughness and extrusion characteristics as well as high gloss surface finish
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 30 hour
30 hour
F<sub>50</sub>; ASTM D1693-B
Melt Flow 0.30 g/10 min
0.30 g/10 min
I<sub>2</sub>; ASTM D1238
28 g/10 min
28 g/10 min
I<sub>21</sub>; ASTM D238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 26.9 MPa
3900 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 1.325 GPa
192.2 ksi
ASTM D790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 130 µm/m-°C

@Temperature 20.0 °C
72.2 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Melting Point 134 °C
273 °F
Petromont
Crystallization Temperature 111 °C
232 °F
Petromont
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °C
165 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Process Sheet Extrusion