Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , LLDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® TS 4016 LDPE and LLDPE Blend - Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene® TS 4016 resin is a mixture of low-density polyethylene (LDPE) with linear low-density polyethylene (LLDPE) designed to meet the needs of the technical films segment for the use of automatic packaging. The formula developed confers to the Trithene® TS 4016 resin easy processability with conventional LDPE extruders, ensuring films with good appearance, thickness uniformity, and excellent weldability. Furthermore, the incorporated additive package brings thermal stability and good slip performance, which are fundamental for offering high productivity rates on the packaging line. The components that form the product Trithene® TS 4016 complies with the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff.Applications: Technical films for the automatic packaging of food products in the form of grains, powder, or farinaceous, such as cereals, sugar, salt, and flours.Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 1.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 460 %
460 %
ASTM D882
Film Elongation at Break, TD 780 %
780 %
ASTM D882
Secant Modulus, MD 0.100 GPa
14.5 ksi
5%; ASTM D882
Secant Modulus, TD 0.110 GPa
16.0 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.10
0.10
ASTM D1894
Elmendorf Tear Strength, MD 7.00 g/micron
178 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 10.5 g/micron
267 g/mil
ASTM D1922
Dart Drop Test 160 g
0.353 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 25.0 MPa
3630 psi
ASTM D882
Film Tensile Strength at Break, TD 22.0 MPa
3190 psi
ASTM D882
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 63 %
63 %
45° - Gardner; ASTM D2457
96 %
96 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 170 - 175 °C
338 - 347 °F
Plasticizing Zone
170 - 180 °C
338 - 356 °F
Mixture Zone
Feed Temperature 160 - 165 °C
320 - 329 °F
Adapter Temperature 175 - 185 °C
347 - 365 °F
Descriptive Properties Value Comments
Proportion LLDPE % 22.5
PTN-570-Q