Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer Petroquimica Triunfo
Trade Name Trithene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petroquimica Triunfo Trithene® TS 8064 LDPE - Packaging Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trithene TS 8064 resin is a low-density polyethylene (LDPE) with a medium molecular weight an excellent processability. Furthermore, this product has good mechanical properties, average transparency, and an additive package with slip, anti-block, and antioxidant agents, which ensure an adequate performance during production lines such as printing, cutting, and welding. This product complies with ASTM standard D1248-IA3 and the requirements of Brazilian and corresponding legislation of Mercosul and it is in conformity with FDA Regulations 21 CFR 177.1520 (c) 2.1, to contact with foodstuff. Applications: Conventional packages and bags for both food and non-food products. Films for general use. Store bags, etc. Resin Properties: Compressed molded plate. Method ASTM D-1928, procedure C. Film obtained on a 50mm blow film line with barrier screw, 25:1 L/D, 1.0mm die gap, 50µm gauge, 2.3:1 BUR.Information provided by Dax Resinas
Physical Properties Metric English Comments
Density 0.920 - 0.926 g/cc
0.0332 - 0.0335 lb/in³
ASTM D1505
Thickness 50.0 microns
1.97 mil
Melt Index of Compound 1.8 - 2.6 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.8 - 2.6 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 12.0 MPa
1740 psi
ASTM D638
Tensile Strength, Yield 11.0 MPa
1600 psi
ASTM D638
Film Elongation at Break, MD 365 %
365 %
ASTM D882
Film Elongation at Break, TD 670 %
670 %
ASTM D882
Elongation at Break 550 %
550 %
ASTM D638
Secant Modulus, MD 0.0970 GPa
14.1 ksi
5%; ASTM D882
Secant Modulus, TD 0.105 GPa
15.2 ksi
5%; ASTM D882
Coefficient of Friction, Dynamic 0.12
0.12
ASTM D1894
Elmendorf Tear Strength, MD 8.40 g/micron
213 g/mil
ASTM D1922
Elmendorf Tear Strength, TD 5.40 g/micron
137 g/mil
ASTM D1922
Dart Drop Test 130 g
0.287 lb
(method A); ASTM D1709
Film Tensile Strength at Break, MD 20.0 MPa
2900 psi
ASTM D882
Film Tensile Strength at Break, TD 18.0 MPa
2610 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 94.0 °C
201 °F
ASTM D1525
Optical Properties Metric English Comments
Haze 9.0 %
9.0 %
ASTM D1003
Gloss 90 %
90 %
@ 60° Gardner; ASTM D2457
Processing Properties Metric English Comments
Processing Temperature 160 - 175 °C
320 - 347 °F
Plasticizing Zone
165 - 180 °C
329 - 356 °F
Mixture Zone
Feed Temperature 150 - 165 °C
302 - 329 °F
Adapter Temperature 170 - 180 °C
338 - 356 °F
Blow-up Ratio (BUR) 3.0
3.0
Recommended