Phenolic - "91LD". Graphite fabric - "WCB"
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 79.98 MPa
11600 psi
Flexural Yield Strength 139 MPa
20200 psi
Flexural Modulus 11.7 GPa
1700 ksi
Compressive Yield Strength 91.0 MPa
13200 psi
Compressive Modulus 14.7 GPa
2130 ksi