Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin  (discontinued **)

Category Polymer , Thermoplastic , Polyolefin
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011.
Physical Properties Metric English Comments
Density 0.903 g/cc
0.0326 lb/in³
Injection molded specimen; ASTM D1505
Melt Flow 3.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
Injection molded specimen; ASTM D2240
Tensile Strength, Yield 8.00 MPa
1160 psi
20 in/min, injection molded, type 1 specimen; ASTM D638
Flexural Modulus 0.0830 GPa
12.0 ksi
Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790
Izod Impact, Notched NB

@Temperature -40.0 °C
NB

@Temperature -40.0 °F
injection molded specimen; ASTM D256
Impact Test 26.0 J

@Temperature -40.0 °C
19.2 ft-lb

@Temperature -40.0 °F
Instrumented, 15 mph; ASTM 3763
Tear Strength 52.0 kN/m
297 pli
Die C, 2 in/min; D1004
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 38.0 °C
100 °F
injection molded specimen; ASTM D648