Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Pinnacle Polymers 5112 C Clarified Random Polypropylene Copolymer, Injection Molding Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Pinnacle Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pinnacle Polymers 5112 C Clarified Random Polypropylene Copolymer, Injection Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties and lot-to-lot consistency.Features: Superior color and processing stabilityLow odorGood flow and set-up behaviorExcellent see-through clarityExcellent lot-to-lot consistencyApplications: Injection molding applications that require high stiffness and excellent clarityCertifications: Pinnacle's polypropylene, as marketed by Pinnacle Polymers Company, in natural, uncolored pellet form complies with appropriate requirements of CFR Title 21, Part 177, Subpart B, Section 177.1520 (c) 1.1a entitled “Olefin Polymers” of the Food Additives Amendment of 1958 to the United States Food, Drug and Cosmetic Act of 1938.Information provided by Pinnacle Polymers.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min
12 g/10 min
Condition L 230/2.16; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa

@Thickness 3.20 mm
4600 psi

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Elongation at Yield 12 %

@Thickness 3.20 mm
12 %

@Thickness 0.126 in
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638
Flexural Modulus 1.31 GPa

@Thickness 3.20 mm
190 ksi

@Thickness 0.126 in
At 1.27 mm/min, 1% secant, injection molded ASTM Type 1 specimen; ASTM D790A
Izod Impact, Notched 0.481 J/cm

@Thickness 3.20 mm,
Temperature 22.8 °C
0.900 ft-lb/in

@Thickness 0.126 in,
Temperature 73.0 °F
injection molded ASTM Type 1 specimen; ASTM D256
Optical Properties Metric English Comments
Haze 8.0 %

@Thickness 1.27 mm
8.0 %

@Thickness 0.0500 in
plaque