Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite Mustang PETG Sheet

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , PETG Copolyester
Manufacturer Plaskolite
Trade Name Mustang
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Mustang PETG Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MUSTANG sheet signage material is continually processed using Eastman Tritan® copolyester, MUSTANG offers superior forming details, improved material distribution and shorter heating and cooling cycles. UV protective layer technology makes MUSTANG an ideal alternative to polycarbonate for indoor and outdoor applications. Flat sheet and roll stock availableData provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.18 g/cc
0.0426 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell M 34
34
ASTM D785
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength 49.6 MPa
7200 psi
ASTM D638
Tensile Modulus 1.59 GPa
230 ksi
ASTM D638
Flexural Strength 65.5 MPa
9500 psi
ASTM D790
Flexural Modulus 1.59 GPa
230 ksi
ASTM D790
Compressive Strength 98.6 MPa
14300 psi
ASTM D695
Izod Impact, Notched 10.1 - 10.7 J/cm

@Thickness <=3.00 mm
19.0 - 20.0 ft-lb/in

@Thickness <=0.118 in
ASTM D256A
Izod Impact Unnotched NB

@Thickness <=3.00 mm
NB

@Thickness <=0.118 in
ASTM D256A
Impact Test >= 22.6 J

@Thickness 5.99 mm,
Temperature 22.8 °C
>= 16.7 ft-lb

@Thickness 0.236 in,
Temperature 73.0 °F
Drop Ball Impact Test, 1 inch dart
>= 22.6 J

@Thickness 5.99 mm,
Temperature -17.8 °C
>= 16.7 ft-lb

@Thickness 0.236 in,
Temperature 0.000 °F
Drop Ball Impact Test, 1 inch dart
Thermal Properties Metric English Comments
CTE, linear 70.2 µm/m-°C

@Temperature -34.4 - -1.11 °C
39.0 µin/in-°F

@Temperature -30.0 - 30.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.0 °C
194 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 85 %
85 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 154 - 182 °C
310 - 360 °F
Forming Temp
Descriptive Properties Value Comments
Flammability B2
Users viewing this material also viewed the following: