Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Gamma Radiation Resistant, Molded , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite
Trade Name Optix®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CA-1000 IG Clear High Impact Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact acrylic resin, injection molding and extrusion gradeApplications: A premium impact acrylic resin particularly suited for medical and food uses. This resin offers the best impact resistance and fracture toughness and is suited for Gamma irradiation treatment. Meets FDA CFR-21 Sec 177.1010 for food use. Meets USP Plastic Class VI for medical use.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Melt Flow 1.6 g/10 min
1.6 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 40.0 MPa
5800 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Modulus of Elasticity 1.38 GPa
200 ksi
ASTM D638
Flexural Strength 46.9 MPa
6800 psi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Gardner Impact 7.34 J
5.42 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 78.0 °C
172 °F
ASTM D648
Vicat Softening Point 100 °C
212 °F
Rate A, ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90.8 %
90.8 %
ASTM D1003
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved