Plaskolite Optix® DA Digital Acrylic Sheet

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Sheet
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® DA Digital Acrylic Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides superior strength and is available in a variety of sizes and thicknesses.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.40 %
0.40 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 95
95
ASTM D785
Tensile Strength 76.05 MPa
11030 psi
ASTM D638
Elongation at Break 5.8 %
5.8 %
ASTM D638
Tensile Modulus 3.38 GPa
490 ksi
ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 3.38 GPa
490 ksi
ASTM D790
Izod Impact, Notched 0.149 J/cm
0.280 ft-lb/in
Milled Notch; ASTM D256
0.214 J/cm
0.400 ft-lb/in
Molded Notch; ASTM D256
Tensile Impact Strength 42.0 kJ/m²
20.0 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature -34.4 - -1.11 °C
30.0 µin/in-°F

@Temperature -30.0 - 30.0 °F
ASTM D696
Thermal Conductivity 0.130 W/m-K
0.900 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 149 - 157 °C
300 - 315 °F
Maximum Service Temperature, Air 76.7 - 87.8 °C
170 - 190 °F
Continuous
Deflection Temperature at 0.46 MPa (66 psi) 97.2 °C
207 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ASTM D648
Softening Point 98.9 - 104 °C
210 - 220 °F
Flame Spread 25.88 mm/min
1.019 in/min
ASTM D635
Flame Spread Index 115
115
ASTM E84
Shrinkage <= 5.0 %
<= 5.0 %
ASTM D702
Optical Properties Metric English Comments
Refractive Index 1.49
1.49
ASTM D542
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 92 %
92 %
ASTM D1003
Descriptive Properties Value Comments
Flammability B2
Self Ignition Temperature 833°F
ASTM D1929
Smoke Developed Index 550
ASTM E84