Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plaskolite PETG Mirror Sheet

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Plaskolite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite PETG Mirror Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Versatile fabrication properties with good impact strength, good design flexibility, and speed of fabrication.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
ASTM D638
Elongation at Break 75 %
75 %
0.3 cm thick
Tensile Modulus 2.10 GPa
305 ksi
ASTM D638
Flexural Yield Strength 77.0 MPa
11200 psi
ASTM D790
Flexural Modulus 2.10 GPa
305 ksi
ASTM D790
Gardner Impact 34.0 J
25.1 ft-lb
No Break
Thermal Properties Metric English Comments
CTE, linear 54.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
30.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648
Vicat Softening Point 82.0 °C
180 °F
ASTM D1525
Electrical Properties Metric English Comments
Electrical Resistivity 6.00e+15 ohm-cm
6.00e+15 ohm-cm
ASTM D257
Dielectric Constant 3.46

@Frequency 100 Hz
3.46

@Frequency 100 Hz
ASTM D150
Dielectric Strength 17.0 kV/mm
432 kV/in
ASTM D149
Users viewing this material also viewed the following: