Material Notes:
Better strength, security, and flame resistance than PETG mirror sheet.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Estimated by MatWeb.
Water Absorption 0.35 %
0.35 %
ASTM D570
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 65.0 MPa
9430 psi
ASTM D638
Tensile Strength, Yield 58.0 MPa
8410 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Tensile Modulus 2.30 GPa
334 ksi
ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
ASTM D790
Compressive Yield Strength 86.0 MPa
12500 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature -18.0 - 38.0 °C
38.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648