Material Notes:
VIVAK offers a balance of physical properties and ease of fabrication. It is ideally suited for complex parts requiring fabrication, including deep thermoforming draws and precise molded-in details. It can be easily decorated by painting, silk screening or hot stamping. VIVAK is heavily used in the POP display and store fixture industries. VIVAK PETG is produced using resin that complies with FDA requirements for food contact applications. VIVAK is a transparent copolyester that offers a unique balance of physical properties and ease of fabrication.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.2 %
0.2 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D285
Tensile Strength 53.1 MPa
7700 psi
ASTM D638
Tensile Modulus 2.208 GPa
320.3 ksi
ASTM D638
Flexural Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.14 GPa
310 ksi
ASTM D790
Compressive Strength 55.2 MPa
8000 psi
ASTM D695
Shear Strength 62.1 MPa
9000 psi
ASTM D732
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature -34.4 - -1.11 °C
38.0 µin/in-°F

@Temperature -30.0 - 30.0 °F
ASTM D696
Thermal Conductivity 0.225 W/m-K
1.56 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 73.3 °C
164 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 69.4 °C
157 °F
ASTM D648
Glass Transition Temp, Tg 81.1 °C
178 °F
ASTM D3418
Flammability, UL94 HB
HB
Flame Spread 1.52 mm/min
0.0600 in/min
ASTM D635
Flame Spread Index 85
85
ASTM E84
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
nD; ASTM D542
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 86 %
86 %
ASTM D1003
Electrical Properties Metric English Comments
Dielectric Constant 2.4

@Frequency 1.00e+6 Hz
2.4

@Frequency 1.00e+6 Hz
ASTM D150
2.6

@Frequency 1000 Hz
2.6

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 16.1 kV/mm
410 kV/in
ASTM D149
Descriptive Properties Value Comments
Self Ignition Temperature 880°F
ASTM D1929
Smoke Developed Index 450
ASTM E84