Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Impact Modified, Molded
Manufacturer Plaskolite West, Inc.
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite West Optix® CA-1000 E Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Extrusion Grade Pellets. Excellent blend stock material for impact applications.
Physical Properties Metric English Comments
Density 1.16 g/cc
0.0419 lb/in³
ASTM D792
Melt Flow 1.1 g/10 min
1.1 g/10 min
Condition 230/3.8; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 45.0 MPa
6530 psi
ASTM D638
Elongation at Break 14.2 %
14.2 %
ASTM D638
Modulus of Elasticity 1.80 GPa
261 ksi
ASTM D638
Flexural Strength 61.0 MPa
8850 psi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Gardner Impact 6.30 J
4.65 ft-lb
ASTM D3029 GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
ASTM D648
Vicat Softening Point 108 °C
226 °F
ASTM D1525
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Transmission, Visible 90.7 %
90.7 %
Luminous Transmittance, ASTM D1003