Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Mineral Reinforced
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTALEN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTALEN® PQ 81 T 10 Polypropylene reinforced with mineral filler.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PP for injection molding with the content of 10% mineral filler, impact modified. Delivered in black color.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
STN EN ISO 1183-1
Filler Content 10 %
10 %
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 27.0 MPa
3920 psi
STN EN ISO 527-2
Elongation at Break 5.8 %
5.8 %
STN EN ISO 527-2
Tensile Modulus 2.15 GPa
312 ksi
STN EN ISO 527-2
Flexural Strength 27.0 MPa
3920 psi
STN EN ISO 178
Flexural Modulus 1.86 GPa
270 ksi
STN EN ISO 178
Charpy Impact Unnotched 1.60 J/cm²

@Temperature -20.0 °C
7.61 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
4.60 J/cm²

@Temperature 23.0 °C
21.9 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.120 J/cm²

@Temperature -20.0 °C
0.571 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.230 J/cm²

@Temperature 23.0 °C
1.09 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Processing Properties Metric English Comments
Melt Temperature 220 - 250 °C
428 - 482 °F
Mold Temperature 40.0 - 50.0 °C
104 - 122 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Descriptive Properties Value Comments
Color Black