Material Notes:
Basic type PA66 for injection molding, heat stabilized, modified for general use, with excellent manufacturing properties. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools, toys. Delivered in the black mode.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
STN EN ISO 1183-1
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
STN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm
0.019 in/in
STN EN ISO 294-4
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 275 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 527 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
STN EN ISO 527-2
Elongation at Break 3.5 %
3.5 %
STN EN ISO 527-2
Tensile Modulus 3.50 GPa
508 ksi
STN EN ISO 527-2
Flexural Strength 95.0 MPa
13800 psi
STN EN ISO 178
Flexural Modulus 2.90 GPa
421 ksi
STN EN ISO 178
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
STN EN ISO 179
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.350 J/cm²

@Temperature 23.0 °C
1.67 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
0.350 J/cm²

@Temperature -20.0 °C
1.67 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
STN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
STN EN ISO 75-2 (A)
Vicat Softening Point 250 °C
482 °F
STN EN ISO 306
Flammability, UL94 V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in
Glow Wire Test 960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
STN EN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 240 - 260 °C
464 - 500 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.25 %
0.25 %
STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Descriptive Properties Value Comments
Color Black