Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom PLASTAMID® 66 GF 35 TS 002 PA66 reinforced with glass fiber, heat stabilized

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Heat Stabilized
Manufacturer Plastcom spol. s r.o.
Trade Name PLASTAMID®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom PLASTAMID® 66 GF 35 TS 002 PA66 reinforced with glass fiber, heat stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PA66 for injection molding, reinforced with 35 % glass fiber, heat stabilized, used in automotive, engineering and electrical industry, eg. intake pipes, cylinder heads, induction coils, carrying parts in the motor area. Application: hobby tools, gears, covers of electric tools, cooling water distribution in the automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
STN EN ISO 1183-1
Filler Content 35 %
35 %
Linear Mold Shrinkage 0.0071 cm/cm
0.0071 in/in
STN EN ISO 294-4
Linear Mold Shrinkage, Transverse 0.0105 cm/cm
0.0105 in/in
STN EN ISO 294-4
Melt Flow 1.5 g/10 min

@Load 0.325 kg,
Temperature 275 °C
1.5 g/10 min

@Load 0.716 lb,
Temperature 527 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 180 MPa
26100 psi
STN EN ISO 527-2
Elongation at Break 2.0 %
2.0 %
STN EN ISO 527-2
Tensile Modulus 10.0 GPa
1450 ksi
STN EN ISO 527-2
Flexural Strength 240 MPa
34800 psi
STN EN ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
STN EN ISO 178
Charpy Impact Unnotched 5.50 J/cm²

@Temperature 23.0 °C
26.2 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
5.50 J/cm²

@Temperature -20.0 °C
26.2 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
Charpy Impact, Notched 0.900 J/cm²

@Temperature -20.0 °C
4.28 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
STN EN 11357-1
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
STN EN ISO 75-2 (A)
Vicat Softening Point 240 °C
464 °F
STN EN ISO 306
Flammability, UL94 HB
HB
Glow Wire Test 650 °C

@Thickness 3.00 mm
1200 °F

@Thickness 0.118 in
STN EN 60695-2-12
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C

@Time 14400 sec
176 °F

@Time 4.00 hour
Moisture Content 0.15 %
0.15 %
STN EN ISO 3344
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi
Descriptive Properties Value Comments
Color Black