Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.915 g/cc
0.0331 lb/in³
Linear Mold Shrinkage 0.021 cm/cm
0.021 in/in
Linear Mold Shrinkage, Transverse 0.0194 cm/cm
0.0194 in/in
Melt Flow 0.50 g/10 min

@Load 0.325 kg,
Temperature 270 °C
0.50 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.0 MPa
3630 psi
Elongation at Break 250 %
250 %
Tensile Modulus 1.45 GPa
210 ksi
Flexural Strength 35.0 MPa
5080 psi
Flexural Modulus 1.30 GPa
189 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Charpy Impact, Notched 1.40 J/cm²

@Temperature -20.0 °C
6.66 ft-lb/in²

@Temperature -4.00 °F
9.00 J/cm²

@Temperature 23.0 °C
42.8 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
Vicat Softening Point 150 °C
302 °F
B
Flammability, UL94 V-2
V-2
Glow Wire Test 960 °C
1760 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
Dielectric Strength 24.0 kV/mm
610 kV/in
Comparative Tracking Index 450 V
450 V
Processing Properties Metric English Comments
Melt Temperature 180 - 210 °C
356 - 410 °F