Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Glass Fiber Filler
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PH 49 GF 25 PP, 25% glass fibre, mod. of mech. properties.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 25 % glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP. Applied in all industry branches. Increased strength, toughness, modulus in tension due to the modification. Delivered in natural and in the full RAL colour scale.Moderately increased toughness and lower MFI in comparison with PH 69 GF 30.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Linear Mold Shrinkage 0.0072 cm/cm
0.0072 in/in
Linear Mold Shrinkage, Transverse 0.0085 cm/cm
0.0085 in/in
Melt Flow 4.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
4.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 5.70 GPa
827 ksi
Flexural Strength 112 MPa
16200 psi
Flexural Modulus 5.45 GPa
790 ksi
Charpy Impact Unnotched 4.30 J/cm²

@Temperature -20.0 °C
20.5 ft-lb/in²

@Temperature -4.00 °F
4.80 J/cm²

@Temperature 23.0 °C
22.8 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.700 J/cm²

@Temperature -20.0 °C
3.33 ft-lb/in²

@Temperature -4.00 °F
1.00 J/cm²

@Temperature 23.0 °C
4.76 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
Vicat Softening Point 162 °C
324 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 40.0 - 80.0 °C
104 - 176 °F
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi