Material Notes:
FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
Linear Mold Shrinkage 0.0181 cm/cm
0.0181 in/in
Linear Mold Shrinkage, Transverse 0.0193 cm/cm
0.0193 in/in
Melt Flow 25 g/10 min

@Load 0.325 kg,
Temperature 270 °C
25 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 34.0 MPa
4930 psi
Elongation at Break 150 %
150 %
Tensile Modulus 1.40 GPa
203 ksi
Flexural Strength 40.0 MPa
5800 psi
Flexural Modulus 1.30 GPa
189 ksi
Charpy Impact Unnotched 3.20 J/cm²

@Temperature -20.0 °C
15.2 ft-lb/in²

@Temperature -4.00 °F
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
Deflection Temperature at 1.8 MPa (264 psi) 80.0 °C
176 °F
Vicat Softening Point 150 °C
302 °F
B
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi