Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled , Nylon 66, 40% Glass Fiber Filled , Nylon 66, Heat Stabilized
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 66
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 66 GF 35 HTS PA66, 355% glass fibre, combined stability.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 66 for injection moulding, chemically reinforced with 35% glass fibre, heat stabilized and stabilized against hydrolysis. Used for cooling water systems in the automotive industry. Delivered in black.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
Viscosity Measurement 0.40 - 0.60
0.40 - 0.60
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Melt Flow 1.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
1.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 200 MPa
29000 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 11.3 GPa
1640 ksi
Flexural Strength 275 MPa
39900 psi
Flexural Modulus 9.80 GPa
1420 ksi
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
8.00 J/cm²

@Temperature -20.0 °C
38.1 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 1.10 J/cm²

@Temperature -20.0 °C
5.23 ft-lb/in²

@Temperature -4.00 °F
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 250 °C
482 °F
Vicat Softening Point 250 °C
482 °F
B
Flammability, UL94 HB
HB
Glow Wire Test 650 °C
1200 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Dielectric Strength 40.0 kV/mm
1020 kV/in
Comparative Tracking Index 400 V
400 V
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 60.0 - 90.0 °C
140 - 194 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi