Material Notes:
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Viscosity Measurement 1.8 - 1.83
1.8 - 1.83
Linear Mold Shrinkage 0.018 cm/cm
0.018 in/in
Linear Mold Shrinkage, Transverse 0.0183 cm/cm
0.0183 in/in
Melt Flow 1.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
1.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.0 MPa
5800 psi
Elongation at Break 50 %
50 %
Tensile Modulus 0.950 GPa
138 ksi
Flexural Strength 45.0 MPa
6530 psi
Flexural Modulus 0.800 GPa
116 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Charpy Impact, Notched 4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
Deflection Temperature at 1.8 MPa (264 psi) 43.0 °C
109 °F
Vicat Softening Point 154 °C
309 °F
B
Processing Properties Metric English Comments
Melt Temperature 280 - 300 °C
536 - 572 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi