Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant

Category Polymer , Thermoplastic , Nylon , Nylon 6/66 , Nylon 66/6, 30% Glass Fiber Reinforced
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVAMID 6/66
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94 V0 at 0,8 mm, glow wire at 960°C, CTI 650. Application for the electrical industry: protectors, coil forms, covers, terminals. Delivered in natural and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
Viscosity Measurement 0.40 - 0.52
0.40 - 0.52
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Linear Mold Shrinkage, Transverse 0.0052 cm/cm
0.0052 in/in
Melt Flow 2.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
2.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 195 MPa
28300 psi
Elongation at Break 2.0 %
2.0 %
Tensile Modulus 10.0 GPa
1450 ksi
Flexural Strength 245 MPa
35500 psi
Flexural Modulus 8.75 GPa
1270 ksi
Charpy Impact Unnotched 7.50 J/cm²

@Temperature -20.0 °C
35.7 ft-lb/in²

@Temperature -4.00 °F
8.50 J/cm²

@Temperature 23.0 °C
40.4 ft-lb/in²

@Temperature 73.4 °F
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
1.10 J/cm²

@Temperature 23.0 °C
5.23 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 262 °C
504 °F
Deflection Temperature at 1.8 MPa (264 psi) 245 °C
473 °F
Vicat Softening Point 252 °C
486 °F
B
Flammability, UL94 V-0

@Thickness 0.800 mm
V-0

@Thickness 0.0315 in
Glow Wire Test 960 °C
1760 °F
at 3 mm
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
Dielectric Strength 60.0 kV/mm
1520 kV/in
Comparative Tracking Index 650 V
650 V
Processing Properties Metric English Comments
Melt Temperature 270 - 300 °C
518 - 572 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.15 %
0.15 %
Injection Pressure 70.0 - 100 MPa
10200 - 14500 psi
Users viewing this material also viewed the following: