Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVASTER® C FRU 2 PBT, flame retarder

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT) , Polybutylene Terephthalate (PBT), Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVASTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVASTER® C FRU 2 PBT, flame retarder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesPC with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, cylindrical or other hole products. Application in engineering, electrical and automotive industry. High mechanical properties also in conditioned state. Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0065 cm/cm
0.0065 in/in
Melt Flow 15 g/10 min

@Load 0.325 kg,
Temperature 270 °C
15 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 5.0 %
5.0 %
Tensile Modulus 2.70 GPa
392 ksi
Flexural Strength 100 MPa
14500 psi
Flexural Modulus 2.60 GPa
377 ksi
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
NB

@Temperature -20.0 °C
NB

@Temperature -4.00 °F
Thermal Properties Metric English Comments
Melting Point 240 °C
464 °F
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
Vicat Softening Point 110 °C
230 °F
B
Flammability, UL94 V-0

@Thickness 1.00 mm
V-0

@Thickness 0.0394 in
Glow Wire Test 960 °C
1760 °F
at 1 mm
Electrical Properties Metric English Comments
Comparative Tracking Index 250 V
250 V
Processing Properties Metric English Comments
Melt Temperature 240 - 270 °C
464 - 518 °F
Mold Temperature 80.0 - 90.0 °C
176 - 194 °F
Drying Temperature 120 °C
248 °F
Dry Time 4 hour
4 hour
Moisture Content 0.050 %
0.050 %
Injection Pressure 60.0 - 100 MPa
8700 - 14500 psi
Copyright © lookpolymers.com All Rights Reserved