PlastiComp Complet® LGF40-PEI Polyetherimide, 40% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyetherimide (PEI) , Polyetherimide (PEI), 40% Glass Fiber
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF40-PEI Polyetherimide, 40% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Filler Content 40 %
40 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 181 MPa
26300 psi
ASTM D-638
Elongation at Break 1.4 %
1.4 %
ASTM D-638
Tensile Modulus 15.172 GPa
2200.5 ksi
ASTM D-638
Flexural Strength 252 MPa
36500 psi
ASTM D-790
Flexural Modulus 15.172 GPa
2200.5 ksi
ASTM D-790
Izod Impact, Unnotched 6.46 J/cm
12.1 ft-lb/in
ASTM D-4812