PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 50% Carbon Fiber Filled
Manufacturer PlastiComp
Trade Name Velocity®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Velocity® LCF50-PA66 High Flow Nylon 66, 50% Long Carbon Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D-792
Filler Content 50 %
50 %
Long Carbon Fiber
Mechanical Properties Metric English Comments
Tensile Strength 310 MPa
45000 psi
ASTM D-638
Elongation at Break 1.0 %
1.0 %
ASTM D-638
Tensile Modulus 40.0 GPa
5800 ksi
ASTM D-638
Flexural Strength 497 MPa
72100 psi
ASTM D-790
Flexural Modulus 29.31 GPa
4251 ksi
ASTM D-790
Izod Impact, Notched 1.82 J/cm
3.41 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 7.21 J/cm
13.5 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 252 °C
486 °F
ASTM D-648