Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 71MR Mineral-Reinforced Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good heat and chemical resistance.Applications: Bike componentsFuel capsAutomotive componentsStandard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.60 %
0.60 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0065 cm/cm

@Thickness 3.17 mm
0.0065 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 88.3 MPa
12800 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 225 °C
437 °F
ASTM D648