Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Calcium Carbonate (CaCO3) Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® C-20 20% Calcium Carbonate-Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® C series compounds are homopolymer polypropylene resins reinforced with fine particle size calcium carbonate. They combine high impact with stiffness, heat aging, good colorability, resistance to environmental stress-cracking, good surface and low mold shrinkage.Applications: AppliancesElectrical componentsHousewaresToysAutomotiveUtility products Standard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792
Filler Content 20 %
20 %
ASTM D2584
Linear Mold Shrinkage 0.010 cm/cm

@Thickness 1.59 mm
0.010 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength at Break 27.6 MPa
4000 psi
ASTM D638
Flexural Modulus 1.93 GPa
280 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.400 J/cm
0.750 ft-lb/in
At 73°F; ASTM D256
Izod Impact, Unnotched 6.41 J/cm
12.0 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 0.983 J
0.725 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C
210 °F
ASTM D648