Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 40% Glass Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPC-40 40% Glass-Reinforced Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycarbonate line an excellent choice for electrical, appliance and hardware applications. Standard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.52 g/cc
0.0549 lb/in³
ASTM D792
Filler Content 40 %
40 %
ASTM D2584
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm

@Thickness 1.59 mm
0.0010 - 0.0020 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 12 - 20 g/10 min
12 - 20 g/10 min
300/1.2; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell M 91
91
ASTM D785
Tensile Strength at Break 157 MPa
22700 psi
ASTM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Tensile Modulus 11.0 GPa
1600 ksi
ASTM D790
Flexural Strength 185 MPa
26800 psi
ASTM D790
Flexural Modulus 9.31 GPa
1350 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.961 J/cm
1.80 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C
295 °F
ASTM D648
Flammability, UL94 HB
HB
Users viewing this material also viewed the following: