Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Glass Fiber Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPP-20 20% Glass-Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuous temperature. Other benefits include reduced distortion under long-term stress.Applications: AppliancesElectrical componentsAutomotiveUtility productsStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Filler Content 20 %
20 %
ASTM D2584
Linear Mold Shrinkage 0.0030 cm/cm

@Thickness 1.59 mm
0.0030 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 44.8 MPa
6500 psi
ASTM D638
Flexural Strength 56.5 MPa
8200 psi
ASTM D638
Flexural Modulus 3.003 GPa
435.5 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 0.678 J
0.500 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 142 °C
288 °F
ASTM D648