Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastxWorld CEVIAN® A2603 15% GF PA/ABS Alloy, Conditioned

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced , Nylon
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® A2603 15% GF PA/ABS Alloy, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property data is for samples equilibrium moisture (1.1%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hr; ASTM D570
Moisture Absorption at Equilibrium 1.1 %
1.1 %
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm
0.0010 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
Flexural Yield Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 3.24 GPa
470 ksi
ASTM D790
Izod Impact, Notched 1.66 J/cm
3.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 150 °C
302 °F
0.5 inch; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Copyright © lookpolymers.com All Rights Reserved