PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced , Nylon
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® A2606 30% GF PA/ABS Alloy, Conditioned.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Property data is for samples at equilibrium moisture (0.7%)These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hr; ASTM D570
Moisture Absorption at Equilibrium 0.70 %
0.70 %
Linear Mold Shrinkage 0.0010 - 0.0050 cm/cm
0.0010 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 115
115
ASTM D785
Tensile Strength at Break 96.5 MPa
14000 psi
ASTM D638
Elongation at Break 6.0 %
6.0 %
ASTM D635
Flexural Yield Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.65 GPa
820 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 180 °C
356 °F
0.5 inch; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in