PlastxWorld CEVIAN® B1700 PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B1700 PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Unfilled, High Heat ResistantThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ASTM D792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.2 MPa
6700 psi
ASTM 638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Yield Strength 71.7 MPa
10400 psi
ASTM D790
Flexural Modulus 2.28 GPa
330 ksi
ASTM D790
Izod Impact, Notched 0.481 J/cm

@Thickness 3.17 mm
0.900 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
0.25 inch; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
0.25 inch; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in