PlastxWorld CEVIAN® B6524 20% GF PBT/ABS Alloy

Category Polymer , Thermoplastic , ABS Polymer , ABS/Polyester Alloy + GF , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN® B6524 20% GF PBT/ABS Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber and mineral filled, low warpage and flame retarded PBT/ABS.Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.43 g/cc
0.0517 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0025 - 0.0045 cm/cm
0.0025 - 0.0045 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 58.6 MPa
8500 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 97.9 MPa
14200 psi
ASTM D790
Flexural Modulus 5.10 GPa
740 ksi
ASTM D790
Izod Impact, Notched 0.374 J/cm

@Thickness 3.17 mm
0.700 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 116 °C
241 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in