Material Notes:
Inherently Static Dissipative Transparent ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
0.0040 - 0.0070 in/in
ASTM D955
Melt Flow 12 g/10 min

@Load 3.80 kg,
Temperature 230 °C
12 g/10 min

@Load 8.38 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D638
Flexural Yield Strength 73.8 MPa
10700 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 0.908 J/cm

@Thickness 3.17 mm
1.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C
187 °F
0.5 inch; ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Haze 4.2 %
4.2 %
0.125 inches; 10 deg
Transmission, Visible 86 %
86 %
0.125 inches; 10 deg
Electrical Properties Metric English Comments
Surface Resistance 5.00e+13 ohm
5.00e+13 ohm
ASTM D249