PlastxWorld CEVIAN®-N ASG30 SAN resin

Category Polymer , Thermoplastic , SAN Polymer , Styrene Acrylonitrile (SAN), Molded, Glass Reinforced
Manufacturer PlastxWorld, Inc.
Trade Name CEVIAN®-N
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld CEVIAN®-N ASG30 SAN resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Glass fiber reinforced SAN resin. These are typical values and are not intended for specification purposes. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
24 hr; ASTM D570
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm
0.0010 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 121 MPa
17500 psi
ASTM D638
Flexural Yield Strength 147 MPa
21300 psi
ASTM D790
Flexural Modulus 8.811 GPa
1278 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C

@Temperature 20.0 °C
12.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
0.25 inch; ASTM D648