Material Notes:
Glass fiber reinforced and flame retarded PC/ABS alloy.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 78.6 MPa
11400 psi
ASTM D638
Elongation at Break 2.0 %
2.0 %
ASTM D638
Flexural Yield Strength 119 MPa
17200 psi
ASTM D790
Flexural Modulus 3.92 GPa
569 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 6.35 mm
1.10 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 57.6 µm/m-°C

@Temperature 20.0 °C
32.0 µin/in-°F

@Temperature 68.0 °F
ASTM D1525
Deflection Temperature at 1.8 MPa (264 psi) 131 °C
268 °F
0.25 inch; ASTM D648
Flammability, UL94 V-0

@Thickness 1.70 mm
V-0

@Thickness 0.0669 in