PlastxWorld Veroplas PA2002HI Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Impact Grade
Manufacturer PlastxWorld, Inc.
Trade Name Veroplas
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastxWorld Veroplas PA2002HI Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
general purpose, unfilled, high impact modified injection molding gradeInformation provided by PlastxWorld Inc.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM A792
Moisture Absorption at Equilibrium <= 0.17 %
<= 0.17 %
Karl Fischer
Linear Mold Shrinkage 0.025 cm/cm
0.025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.8 MPa
6500 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Yield Strength 57.9 MPa
8400 psi
ASTM D790
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 10.00 J/cm
18.73 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D648
Vicat Softening Point 171 °C
340 °F
ASTM D1525