Plenco 00714 Melamine-Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00714 Melamine-Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E40654. 00714 is available in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.700 g/cc
0.0253 lb/in³
ASTM D1895
Density 1.67 g/cc
0.0603 lb/in³
ASTM D792
Water Absorption 0.22 %
0.22 %
ASTM D570
Linear Mold Shrinkage 0.0036 cm/cm
0.0036 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 74
74
ASTM D785
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ASTM D638
Elongation at Break 0.81 %
0.81 %
ASTM D638
Tensile Modulus 13.3 GPa
1930 ksi
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 11.2 GPa
1620 ksi
ASTM D790
Compressive Strength 167 MPa
24200 psi
ASTM D695
Izod Impact, Notched 0.168 J/cm
0.315 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.218 J/cm²
1.04 ft-lb/in²
ASTM D256
Impact 96
96
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 194 °C
381 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.62 %
0.62 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 7.50e+13 ohm-cm
7.50e+13 ohm-cm
ASTM D247
Dielectric Constant 6.5
6.5
ASTM D150
Dielectric Strength 10.4 kV/mm
264 kV/in
Step by Step; ASTM D149
13.6 kV/mm
345 kV/in
Short Time; ASTM D149
Dissipation Factor 0.047
0.047
ASTM D150
Arc Resistance 186 sec
186 sec
ASTM D495
Comparative Tracking Index 425 V
425 V
ASTM D3638
Users viewing this material also viewed the following: