Category Polymer , Thermoset , Melamine , Melamine-Phenolic Copolymer , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 00755 Melamine-Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755 is available only in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.36 %
0.36 %
ASTM D570
Linear Mold Shrinkage 0.0042 cm/cm
0.0042 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 71
71
ASTM D785
Tensile Strength, Ultimate 56.0 MPa
8120 psi
ASTM D638
Elongation at Break 0.64 %
0.64 %
ASTM D638
Tensile Modulus 10.0 GPa
1450 ksi
ASTM D638
Flexural Strength 89.0 MPa
12900 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Compressive Strength 165 MPa
23900 psi
ASTM D695
Izod Impact, Notched 0.201 J/cm
0.377 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.221 J/cm²
1.05 ft-lb/in²
ASTM D256
Impact 148
148
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Thermal Conductivity 0.580 W/m-K

@Temperature 100 °C
4.03 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 152 °C
306 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 184 °C
363 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 33 %
33 %
ASTM D2863
Shrinkage 0.89 %
0.89 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.80e+13 ohm-cm
1.80e+13 ohm-cm
ASTM D247
Dielectric Constant 6.5
6.5
ASTM D150
Dielectric Strength 8.50 kV/mm
216 kV/in
Step by Step; ASTM D149
12.0 kV/mm
305 kV/in
Short Time; ASTM D149
Dissipation Factor 0.054
0.054
ASTM D150
Arc Resistance 186 sec
186 sec
ASTM D495
Comparative Tracking Index 425 V
425 V
ASTM D3638