Material Notes:
PLENCO 00755 is a melamine-phenolic copolymer molding compound offering excellent electrical and flame resistant properties. Type ASTM 5948 CMG, and UL recognized under component file E40654. 00755 is available only in brown.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.580 g/cc
0.0210 lb/in³
ASTM D1895
Density 1.60 g/cc
0.0578 lb/in³
ASTM D792
Water Absorption 0.44 %
0.44 %
ASTM D570
Linear Mold Shrinkage 0.0069 cm/cm
0.0069 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 76
76
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 10.2 GPa
1480 ksi
ASTM D638
Flexural Strength 85.0 MPa
12300 psi
ASTM D790
Flexural Modulus 8.60 GPa
1250 ksi
ASTM D790
Compressive Strength 168 MPa
24400 psi
ASTM D695
Izod Impact, Notched 0.191 J/cm
0.358 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.215 J/cm²
1.02 ft-lb/in²
ASTM D256
Impact 99
99
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 186 °C
367 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Shrinkage 0.96 %
0.96 %
240 hr, 105ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.60e+12 ohm-cm
1.60e+12 ohm-cm
ASTM D247
Dielectric Constant 7.3
7.3
ASTM D150
Dielectric Strength 5.80 kV/mm
147 kV/in
Step by Step; ASTM D149
7.70 kV/mm
196 kV/in
Short Time; ASTM D149
Dissipation Factor 0.074
0.074
ASTM D150
Arc Resistance 186 sec
186 sec
ASTM D495
Comparative Tracking Index 475 V
475 V
ASTM D3638