Plenco 05118-T5 Phenolic, Granular, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Mineral/Graphite Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 05118-T5 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 05118-T5 is a mineral and graphite filled novolac phenolic molding compound with PTFE, formulated for bearing seals. 05118 provides for a low coefficient of friction, good wear resistance, very low water absorption, and good dimensional stability under severe exposure. 05118 is available in grey.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.910 g/cc
0.0329 lb/in³
ASTM D1895
Density 1.84 g/cc
0.0665 lb/in³
ASTM D792
Water Absorption 0.044 %
0.044 %
ASTM D570
Linear Mold Shrinkage 0.0034 cm/cm
0.0034 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 61
61
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 0.45 %
0.45 %
ASTM D638
Tensile Modulus 13.9 GPa
2020 ksi
ASTM D638
Flexural Strength 68.0 MPa
9860 psi
ASTM D790
Flexural Modulus 11.7 GPa
1700 ksi
ASTM D790
Compressive Strength 117 MPa
17000 psi
ASTM D695
Izod Impact, Notched 0.162 J/cm
0.303 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.167 J/cm²
0.795 ft-lb/in²
ASTM D256
Impact 61
61
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 210 °C
410 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ASTM D648
Shrinkage 0.057 %
0.057 %
72 hr, 120ºC; ASTM D1299