Plenco 08225 Polyester BMC, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 08225 Polyester BMC, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 08225 is a renumber of PlasGlas 20215. PLENCO 08225 is a 15% glass-filled polyester bulk molding compound characterized as a medium strength electrical grade, but has many outstanding properties that make it suitable for a broad range of applications such as coil bobbins, where assembly and end use environments are particularly strenuous. It is available in bulk or extruded form, natural and black. Other colors available upon request. It is UL recognized under file E40654.Information supplied by Plenco.
Physical Properties Metric English Comments
Density 1.93 g/cc
0.0697 lb/in³
ASTM D792
Water Absorption 0.073 %
0.073 %
ASTM D570
Linear Mold Shrinkage 0.00281 cm/cm
0.00281 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 51
51
ASTM D785
Tensile Strength, Ultimate 47.0 MPa
6820 psi
ASTM D638
Elongation at Break 0.56 %
0.56 %
ASTM D638
Tensile Modulus 14.0 GPa
2030 ksi
ASTM D638
Flexural Strength 113 MPa
16400 psi
ASTM D790
Flexural Modulus 13.3 GPa
1930 ksi
ASTM D790
Compressive Strength 136 MPa
19700 psi
ASTM D695
Izod Impact, Notched 2.89 J/cm
5.41 ft-lb/in
ASTM D256
Charpy Impact, Notched 3.00 J/cm²
14.3 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 236 °C
457 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 273 °C
523 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.00143 %
0.00143 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.20e+16 ohm-cm
2.20e+16 ohm-cm
ASTM D247
Dielectric Constant 4.6
4.6
ASTM D150
Dielectric Strength 10.6 kV/mm
269 kV/in
Step by Step; ASTM D149
12.8 kV/mm
325 kV/in
Short Time; ASTM D149
Dielectric Breakdown 22750 V
22750 V
1hr 120C; ASTM D149
Dissipation Factor 0.0059
0.0059
ASTM D150
Arc Resistance 183 sec
183 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638