Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1500 Polyester, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1500 Polyester, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under component file E40654. 01500 is available in black or tan color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.830 g/cc
0.0300 lb/in³
ASTM D1895
Density 1.86 g/cc
0.0672 lb/in³
ASTM D792
Water Absorption 0.33 %
0.33 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 64
64
ASTM D785
Tensile Strength, Ultimate 34.0 MPa
4930 psi
ASTM D638
Elongation at Break 0.41 %
0.41 %
ASTM D638
Tensile Modulus 12.4 GPa
1800 ksi
ASTM D638
Flexural Strength 66.0 MPa
9570 psi
ASTM D790
Flexural Modulus 10.5 GPa
1520 ksi
ASTM D790
Compressive Strength 147 MPa
21300 psi
ASTM D695
Izod Impact, Notched 0.165 J/cm
0.309 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.180 J/cm²
0.857 ft-lb/in²
ASTM D256
Impact 61
61
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 40.0 - 130 °C
36.1 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.760 W/m-K

@Temperature 100 °C
5.27 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 188 °C
370 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 178 °C
352 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
Oxygen Index 34 %
34 %
ASTM D2863
Shrinkage 0.056 %
0.056 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 4.40e+14 ohm-cm
4.40e+14 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 10.7 kV/mm
272 kV/in
Step by Step; ASTM D149
13.5 kV/mm
343 kV/in
Short Time; ASTM D149
Dielectric Breakdown 20200 V
20200 V
1hr 120C; ASTM D149
Dissipation Factor 0.0259
0.0259
ASTM D150
Arc Resistance 190 sec
190 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638
Users viewing this material also viewed the following: