Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1500 Polyester, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1500 Polyester, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01500 is a general purpose, mineral filled granular polyester molding compound, offering excellent arc and track resistance, and low post shrinkage characteristics. UL recognized under component file E40654. 01500 is available in black or tan color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.840 g/cc
0.0303 lb/in³
ASTM D1895
Density 1.87 g/cc
0.0676 lb/in³
ASTM D792
Water Absorption 0.35 %
0.35 %
ASTM D570
Linear Mold Shrinkage 0.0079 cm/cm
0.0079 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 66
66
ASTM D785
Tensile Strength, Ultimate 42.0 MPa
6090 psi
ASTM D638
Elongation at Break 0.63 %
0.63 %
ASTM D638
Tensile Modulus 10.7 GPa
1550 ksi
ASTM D638
Flexural Strength 75.0 MPa
10900 psi
ASTM D790
Flexural Modulus 10.5 GPa
1520 ksi
ASTM D790
Compressive Strength 148 MPa
21500 psi
ASTM D695
Poissons Ratio 0.31
0.31
ASTM D638
Shear Modulus 4.08 GPa
592 ksi
Calculated
Izod Impact, Notched 0.174 J/cm
0.326 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.181 J/cm²
0.861 ft-lb/in²
ASTM D256
Impact 66
66
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 40.0 - 130 °C
38.9 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 177 °C
351 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 174 °C
345 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
Oxygen Index 35 %
35 %
ASTM D2863
Shrinkage 0.045 %
0.045 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 5.60e+14 ohm-cm
5.60e+14 ohm-cm
ASTM D247
Dielectric Constant 5.1
5.1
ASTM D150
Dielectric Strength 10.3 kV/mm
262 kV/in
Step by Step; ASTM D149
13.1 kV/mm
333 kV/in
Short Time; ASTM D149
Dielectric Breakdown 20000 V
20000 V
1hr 94C; ASTM D149
Dissipation Factor 0.0253
0.0253
ASTM D150
Arc Resistance 224 sec
224 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638