Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1506 Polyester, Briquette, Injection Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1506 Polyester, Briquette, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01506 is a mineral and cellulose filled granular polyester molding compound, with glass fiber reinforcement for improved mechanical strength properties. 01506 offers excellent electrical properties and resistance to chemical degradation from repeated detergent exposure. UL recognized under component file E40654. 01506 is available in beige or taupe color.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.690 g/cc
0.0249 lb/in³
ASTM D1895
Density 1.70 g/cc
0.0614 lb/in³
ASTM D792
Water Absorption 0.151 %
0.151 %
ASTM D570
Linear Mold Shrinkage 0.0058 cm/cm
0.0058 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 61
61
ASTM D785
Tensile Strength, Ultimate 54.0 MPa
7830 psi
ASTM D638
Elongation at Break 1.11 %
1.11 %
ASTM D638
Tensile Modulus 9.90 GPa
1440 ksi
ASTM D638
Flexural Strength 95.0 MPa
13800 psi
ASTM D790
Flexural Modulus 9.20 GPa
1330 ksi
ASTM D790
Compressive Strength 131 MPa
19000 psi
ASTM D695
Izod Impact, Notched 0.292 J/cm
0.547 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.255 J/cm²
1.21 ft-lb/in²
ASTM D256
Impact 207
207
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 76.0 µm/m-°C

@Temperature 40.0 - 130 °C
42.2 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 192 °C
378 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 226 °C
439 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 3.00 mm
V-1

@Thickness 0.118 in
Oxygen Index 32 %
32 %
ASTM D2863
Shrinkage 0.0206 %
0.0206 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 7.60e+14 ohm-cm
7.60e+14 ohm-cm
ASTM D247
Dielectric Constant 4.2
4.2
ASTM D150
Dielectric Strength 11.7 kV/mm
297 kV/in
Step by Step; ASTM D149
13.6 kV/mm
345 kV/in
Short Time; ASTM D149
Dielectric Breakdown 20900 V
20900 V
1hr 120C; ASTM D149
Dissipation Factor 0.019
0.019
ASTM D150
Arc Resistance 191 sec
191 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638