Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 1508 Polyester, Briquette, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Polyester, TS , Thermoset Polyester, Mineral Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 1508 Polyester, Briquette, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 01508 is a mineral filled pelletized polyester molding compound, which offers excellent heat resistance and electrical properties. UL recognized under component file E40654. 01508 is available in gray.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.940 g/cc
0.0340 lb/in³
ASTM D1895
Density 2.08 g/cc
0.0751 lb/in³
ASTM D792
Water Absorption 0.123 %
0.123 %
ASTM D570
Linear Mold Shrinkage 0.0034 cm/cm
0.0034 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 77
77
ASTM D785
Tensile Strength, Ultimate 49.0 MPa
7110 psi
ASTM D638
Elongation at Break 0.55 %
0.55 %
ASTM D638
Tensile Modulus 13.2 GPa
1910 ksi
ASTM D638
Flexural Strength 84.0 MPa
12200 psi
ASTM D790
Flexural Modulus 13.9 GPa
2020 ksi
ASTM D790
Compressive Strength 161 MPa
23400 psi
ASTM D695
Poissons Ratio 0.284
0.284
ASTM D638
Shear Modulus 5.14 GPa
746 ksi
Calculated
Izod Impact, Notched 0.241 J/cm
0.451 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.276 J/cm²
1.31 ft-lb/in²
ASTM D256
Impact 115
115
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 40.0 - 130 °C
29.4 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 208 °C
406 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 231 °C
448 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Oxygen Index 47 %
47 %
ASTM D2863
Shrinkage 0.0060 %
0.0060 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+15 ohm-cm
1.30e+15 ohm-cm
ASTM D247
Dielectric Constant 4.8
4.8
ASTM D150
Dielectric Strength 10.2 kV/mm
259 kV/in
Step by Step; ASTM D149
12.3 kV/mm
312 kV/in
Short Time; ASTM D149
Dielectric Breakdown 22500 V
22500 V
ASTM D149
Dissipation Factor 0.0149
0.0149
ASTM D150
Arc Resistance 188 sec
188 sec
ASTM D495
Comparative Tracking Index 600 V
600 V
ASTM D3638