Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Novolac, Woodflour Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2000 Phenolic, Granular, Injection Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under component file E40654. 02000 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.590 g/cc
0.0213 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.32 %
0.32 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 57.0 MPa
8270 psi
ASTM D638
Elongation at Break 0.81 %
0.81 %
ASTM D638
Tensile Modulus 7.60 GPa
1100 ksi
ASTM D638
Flexural Strength 81.0 MPa
11700 psi
ASTM D790
Flexural Modulus 6.80 GPa
986 ksi
ASTM D790
Compressive Strength 198 MPa
28700 psi
ASTM D695
Poissons Ratio 0.36
0.36
ASTM D638
Shear Modulus 2.79 GPa
405 ksi
Calculated
Izod Impact, Notched 0.153 J/cm
0.287 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.179 J/cm²
0.852 ft-lb/in²
ASTM D256
Impact 93
93
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 51.0 µm/m-°C

@Temperature 40.0 - 130 °C
28.3 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Maximum Service Temperature, Air 198 °C
388 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 155 °C
311 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 1.50 mm
V-1

@Thickness 0.0591 in
Oxygen Index 29 %
29 %
ASTM D2863
Shrinkage 0.37 %
0.37 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 2.30e+11 ohm-cm
2.30e+11 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 8.50 kV/mm
216 kV/in
Short Time; ASTM D149
Dissipation Factor 0.058
0.058
ASTM D150
Arc Resistance 134 sec
134 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638