Material Notes:
Two-stage Phenolic. PLENCO 02424 is a black, two stage, general purpose phenolic molding compound. It has a good balance of properties for a general purpose type material. It is used in electrical applications and can be molded by compression, transfer, or injection.Information supplied by Plenco
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Apparent Bulk Density 0.640 g/cc
0.0231 lb/in³
Apparent density per ASTM D1895
Water Absorption 0.31 %
0.31 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
per ATM D955. Post shrinkage is 0.29% at 72hr 120ºC per ASTM D1299.
Mechanical Properties Metric English Comments
Hardness, Rockwell E 86
86
ASTM D785
Tensile Strength, Ultimate 57.9 MPa
8400 psi
ASTM D638
Elongation at Break 0.77 %
0.77 %
ASTM D638
Tensile Modulus 8.45 GPa
1230 ksi
ASTM D638
Flexural Yield Strength 81.1 MPa
11800 psi
ASTM D790
Flexural Modulus 7.53 GPa
1090 ksi
ASTM D790
Compressive Yield Strength 199.7 MPa
28960 psi
ASTM D695
Charpy Impact, Notched 0.190 J/cm²
0.904 ft-lb/in²
ASTM D256
Impact 102
102
J/m Plenco drop ball test
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Heat resistance per ASTM D794
Deflection Temperature at 1.8 MPa (264 psi) 160 °C
320 °F
ASTM D648
Flammability, UL94 V-1

@Thickness 6.10 mm
V-1

@Thickness 0.240 in
Electrical Properties Metric English Comments
Electrical Resistivity 5.33e+11 ohm-cm
5.33e+11 ohm-cm
ASTM D257
Dielectric Constant 5.3

@Frequency 1e+6 Hz
5.3

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 9.00 kV/mm
229 kV/in
Step by Step; ASTM D149
10.4 kV/mm
264 kV/in
Short Time; ASTM D149
Dissipation Factor 0.060

@Frequency 1e+6 Hz
0.060

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 160 sec
160 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638