Plenco 2567 Phenolic, Granular, Compression Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Resole, Wood Filled
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 2567 Phenolic, Granular, Compression Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under component file E40654. 02567 is available in black, brown, or red color. 02567 Black is not intended for electrical insulating applications.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.610 g/cc
0.0220 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.47 %
0.47 %
ASTM D570
Linear Mold Shrinkage 0.0041 cm/cm
0.0041 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 84
84
ASTM D785
Tensile Strength, Ultimate 62.0 MPa
8990 psi
ASTM D638
Elongation at Break 0.87 %
0.87 %
ASTM D638
Tensile Modulus 8.00 GPa
1160 ksi
ASTM D638
Flexural Strength 91.0 MPa
13200 psi
ASTM D790
Flexural Modulus 7.40 GPa
1070 ksi
ASTM D790
Compressive Strength 215 MPa
31200 psi
ASTM D695
Izod Impact, Notched 0.152 J/cm
0.285 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.187 J/cm²
0.890 ft-lb/in²
ASTM D256
Impact 102
102
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
CTE, linear 63.0 µm/m-°C

@Temperature 40.0 - 130 °C
35.0 µin/in-°F

@Temperature 104 - 266 °F
TMA; ASTM E831
Thermal Conductivity 0.370 W/m-K

@Temperature 100 °C
2.57 BTU-in/hr-ft²-°F

@Temperature 212 °F
ASTM E1461
Maximum Service Temperature, Air 203 °C
397 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 185 °C
365 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Oxygen Index 29 %
29 %
ASTM D2863
Shrinkage 0.40 %
0.40 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+13 ohm-cm
3.00e+13 ohm-cm
ASTM D247
Dielectric Constant 5.4
5.4
ASTM D150
Dielectric Strength 9.50 kV/mm
241 kV/in
Step by Step; ASTM D149
12.9 kV/mm
328 kV/in
Short Time; ASTM D149
Dissipation Factor 0.041
0.041
ASTM D150
Arc Resistance 87 sec
87 sec
ASTM D495
Comparative Tracking Index 175 V
175 V
ASTM D3638